Dear All,
Hi,
I have a one PQR with PWHT,Heat treatment cycle is 660 - 665 Deg. C
Temp. and time 95 minutes, and my job Heat treatment cycle 660 - 665
Deg. C. Temp and soking time 40 minutes (min).can i use this pqr for
job.
Thanks
Satish,
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35289] Welding consumable for S355J2WP material
S355 J2 WP is a weathering structural steel It has better atmospheric corrosion resistance. Use E 8018 - W1/W2 Electrodes This is regular...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-