RE: [MW:15223] ER 70S-G has A no ?

Dear ,

Mr. murugam is right .u have to check ur welding consumable chemical composition with QW 442. And it must be A 1

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kavin Murugam
Sent: 04 September 2012 11:13
To: materials-welding@googlegroups.com
Subject: Re: [MW:15216] ER 70S-G has A no ?

 

Dear Deni Rustari,

 

Kindly refer batch certificate and match the chemical composition in accordance to QW442 or record as per mill certificate in PQR.

 

Regards,

Kavin Murugam

0126159644

 

 

From: Deni Rustari <deni.rustari@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, September 3, 2012 2:43 PM
Subject: [MW:15192] ER 70S-G has A no ?



Dear Experts,

 

How to explain that ER-70S-G has A No, because A no for GTAW process is an essential variable,

If we refer to ASME sec II C, SFA 5.18 tabel 1 CHEMICAL COMPOSITION REQUIREMENTS FOR SOLID ELECTRODES AND RODS, for ER70S-G is Not Specified..

 

Thanks for your attention

 

Best Regards

 

Deni Rustari

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...