Saturday, September 1, 2012

Re: [MW:15180] Defects in the MIG welding of F91+F91 -reg

Please check your powersource which you are using for GMAW. There are controls on the powersource for adjusting the crater parameters ! Just adjust the parameters (current/voltage) of crater setting knob and your problem will be solved.
 
 
Regards
 
Prem Nautiyal
Cell: 9769316004
 

--- On Fri, 8/31/12, Sankaran Sp <subasankaran@yahoo.co.in> wrote:

From: Sankaran Sp <subasankaran@yahoo.co.in>
Subject: [MW:15173] Defects in the MIG welding of F91+F91 -reg
To: materials-welding@googlegroups.com
Date: Friday, August 31, 2012, 3:33 PM

Dear friends,

I am working the leading valve manufacturing company in Coimbatore ( INDIA) i ma facing quality issue in the MIG welding of Er 90S-B9.
We have product in ASTM A182- F91 forged steel valve ( Equivalent to C12A casting or P91 pipes),during welding of body+Bonnet we are facing the crack in the crater area.
Our welding parameters are as below:
Joint type = Circumferential Fillet welding, Current = 215 - 235  Amps, V = 25 - 27 Volts, Shielding Gas = Ar+CO2 ( 80+20 % mixture), Gas flow = 20 - 25 LPM, Pre heat temp =  210 - 230 Deg C, Inter pass temp= 320 - 380 Deg C
>After welding ,the joint was inspected by M.P test andcrack found on crater area.
> Removed the welding by turning, then re- test carried out with increased
the post flow timings of shielding gas, but no improvement in the test, same
crack appeared on crater area.

What will be the reason for this defect? Can you suggest me suitable method
to over come this problem?
What will be the reason for this crack?
Kindly send your recommendations to solve this issue.

Advance thanks and regards,
Sankaran.SP
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon