Dear ALL,

While reviewing PWHT chart, I found that for IS 2062 E250 B, 50mm butt joints holding temp found exceed by 10degree (Required 590 deg +- 10 deg and observed 610 deg).
My question is 1) Is it acceptable?
2) what will be the effect on joints by exceeding 10 deg temp out of specified limit?
3) Does code permit to do PWHT again on same joints in specified limit of temp?

Thanks & regards,

Mohd. Sadique Sheikh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...