Re: [MW:14248] Can a ss qualified welder do back welding

Yem,

Absolutely yes. Back welding is not a essential variable as per ASME code. and I guess this allowance is also applicable for any other welding standards.

2012/5/11 mpk mpk <ranmi2007@gmail.com>
Dear Experts,

Can a ss qualified welder do back welding ?

Thank you,

Yem Pee.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
修延飞
Yanfei Xiu
技术中心 焊接室
Tech Center,welding department
山东核电设备制造有限公司
SNPEMC  
地址:中国山东海阳临港产业区
Address:Lingang Industrial Area,Haiyang City,Shandong Province ,PRC
TEL:15967615395


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...