We have 2 x 1000 TPD Sufuric Acid Plants, 750 MTPD Phos Acid Plant, 16x2 MW CPP & Wide HP & LP Stream distribution network.

We are facing Frequent acid , gas , steam leakages.

Any hot tapping procedure , that cal help us to carry out on stream, will be welcome.

Pl. let us know in return mail.

Regds,

akpradhan

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of rafeeqmahadighar rahman
Sent: Saturday, May 05, 2012 2:58 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14190] HOT TAPPING OF LPG PIPE LINES

 

Dear Venkat,

recently we have done the Hot-tap for our project, the hot tap crew & their safety team will assess the area, condition of the site, as well as your emergency contingency plan based on the risk assessment.

you need to have basically following in your hand.

1) Hot-Tap package (hot-tap procedure, welding procedure, hot-tap calculation, UT reading, ISO, P&ID, MTO etc).

2) Emergency contingency plan.

3) Split tee hydro test reports.

4) Spool hydro test report. etc.

 

Warm Regards'

Rafeeq Ur Rahman

 

From: N VENKATESWARA PRASAD <weldengr.velosi@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Thursday, 3 May 2012 11:16 AM
Subject: [MW:14177] HOT TAPPING OF LPG PIPE LINES



Dear Friends,

 

We are planning to do  hot tapping of LPG pipe lines with wall thcikness of 9 mm.  Does any body have experience with the same, please share.  We have qualified the procedure, but  there are apprenhensions regarding safety in hot tapping of LPG pipe lines

 

Regards

 

Venkat

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

1 comment:

S. Wani said...

Please contact us for more details. We will provide you all details & service in this regard.

Regards / S. Wani

shw@conmatindia.com

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...