Wednesday, May 2, 2012

Re: [MW:14172] API 650 - telltale hole in RF pad

Hi,
 
This is really intresting Question, for pipe when we are adding R-Pad the weep hole shall be on the opposite side of crotch.
 
Regards,
Srinivas

On Sun, Apr 29, 2012 at 2:55 PM, M S <striarc@gmail.com> wrote:
Dear Experts,


As per API 650, telltale hole shall be located substatially on the horizontal centerline. Could you please explain the reason. What will be the effect if the tellhole located at other locations?

Regards.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Ohm Guru Namasivaya

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone