Dear sir,
 
 
pl give clarification, Regarding WPS, My WPS is Galvanised coating pipe welded with electrode root 6010 & final 6013.while doing WPS coating was removed & wps was passed.
 
 
 
MY QUESTION
 
1Q.The same WPS using in fire fighting system,it is necessary to remove the galvanised coating on prodution side also?
 
2Q. If really want to remove the galvanised coating , what is the different ways of procedures to remove the galvanised coating on pipes?
 
3Q.If not necessary to remove the galvanised coating , pl suggest acceptance code for this issue?
 
 
regards,
 
ch.srinivasarao.
LARSEN & TOUBRO.
MUMBAI
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...