Re: [MW:13333] Stainless steel plate rolling

Hi
 
You can use the same rolling machine..
Only care you should take while rolling SS material is that the rolls should be wrapped with a "felt"- any matted fabric inorder to avoid Fe contamination.
 
Regards
 
Prem Nautiyal


--- On Tue, 12/27/11, rinshu <rinshad043@gmail.com> wrote:

From: rinshu <rinshad043@gmail.com>
Subject: [MW:13330] Stainless steel plate rolling
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Tuesday, December 27, 2011, 6:53 PM

Dear all,


Can anybody help me on the rolling of austenitic stainless steel plate
for the pressure vessel,we are having facilities for the rolling of
carbon steel plate. Can we use the same rolling machine? Need to have
any precaution before rolling in the same machine ?


Regards

Rinshad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

1 comment:

swetang said...

can any body guide me what is methods for SS Shell After bending and welding of shell joint due to to radiation welding joint we have to pit for making starightning, which is the method with photos

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...