[MW:13243] IMPACT TEST -SUB SIZE

Hi,

 

Now we are qualifying two new PQR for new project for less base metal

thick. (9mm). Code AWS D1.1

 

ROOT / HOT Pass              -GTAW (deposited 4mm)

Fill/Cap                                - SMAW (deposited 5mm)

 

We need to perform the impact test as per Client Welding spec for each process.

In this case, we have to go for Sub size with temperature reduction.

 

Client Welding spec requirement is minimum - 29 °C. 

 

If I go with 10x5mm sub size, I need to reduce 11.1 °C  and test to be

done at -40.1°C. (  -29 -11.1) 

Then Joule value will considered as per ASTM 370,16 J from the below

second table.

 

Is it correct ?

 

With Kind Regards,

 

S.Elumalai.

******************************************************************************************
CONFIDENTIALITY NOTICE
This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...