[MW:12632] Procedure for welding of sailhard material..........

Dear experts,
Could any one solve my doubts.........
     1)What are the welding consumables to be used for SAILHARD material?
     2)what is the procedure to weld SAILHARD plate material more than 10
         mm thick?               

--
THANKS & REGARDS
 
KALYAN VVV
WELDING ENGINEER
HYDERABAD

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...