Dear Experts
 
I'm not sure if either AWS D1.1 and/or ASME Sect. IX ( both year 2010 )prohibits using PQR qualified to other codes.
However ASME do not have any provision for 6GR Position but only recognize "special position" in QW-303.3.
 
According to AWS D1.1-Note "d" in Table 4.10 & Note "c" in Table 4.1-PQT   Pls refer attached AWS Interpretation

I need all you guidance best method on:-

1 - Qualifying Welding Procedure Qualification to AWS D1.1 & ASME Sect IX in one  Test. ( with/without Impact Energy value ).
2 - Welder Qualification using PQR qualified to AWS D1.1 & ASME Sect IX
3 - Propose to use Dual Codes Qualification in one Welder/Welding Operator's Certificate.

And also want to welders using PQR qualified to AWS D1.1 & ASME Sect IX.
Weld Process - SMAW , FCAW . GMAW ,  GTAW , SMAW/FCAW, GTAW/SMAW....etc

My purpose.
1 - Reduce number of PQR and Welder Qualification
2 - Minimize Certification documenation and necessary follow-up
3 - Muliti-purpose welder/welding operator


With Warmest Regards

Ganesan
 H/P - 65 9189 6531 
 
"Happiness keeps you Sweet, 
Trials keep you Strong,
Sorrow keeps you Human,
Failure keeps you humble
and Success keeps you glowing, 
but only Faith & Attitude Keeps you going.. "
 
 
 




 

 








 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...