RE: [MW:10541] 3F & 4F position in single test coupon

Yes, it is possible, see QW-461.9 Plate – fillet. ASME 2010 section IX

Regards

 

Di Prinzio, Juan Carlos

 

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de Fitria Rahman
Enviado el: jueves, 31 de marzo de 2011 1:56
Para: materials-welding@googlegroups.com
Asunto: Re: [MW:10538] 3F & 4F position in single test coupon

 

No it can not. Please refer to QW-461.9 for BOILER AND PRESSURE VESSEL code and Table 4.9 for ASW D11.

I suggest you to qualify welder in 6G position.


rgds

2011/3/31 Ramesh Barot <rameshnbarot@yahoo.com>

Dear Sir,

Can we qualify welderin single test coupon by root in 3F position and other passes by 4F position to qualifyall position. Testcoupon size is 12mm thk and 300mm long.

Please give reference also.

Thanks to all for your valuable inputs.Thanks,
With Best Regards,
Ramesh Barot

Cell+919978917399

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

__________ Información de ESET Smart Security, versión de la base de firmas de virus 6002 (20110331) __________

 

ESET Smart Security ha comprobado este mensaje.

 

http://www.eset.com



__________ Información de ESET Smart Security, versión de la base de firmas de virus 6002 (20110331) __________

ESET Smart Security ha comprobado este mensaje.

http://www.eset.com

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...