Thursday, March 31, 2011

Re: [MW:10538] 3F & 4F position in single test coupon

No it can not. Please refer to QW-461.9 for BOILER AND PRESSURE VESSEL code and Table 4.9 for ASW D11.

I suggest you to qualify welder in 6G position.


rgds

2011/3/31 Ramesh Barot <rameshnbarot@yahoo.com>

Dear Sir,

 

Can we qualify welder in single test coupon by root in 3F position and other passes by 4F position to qualify all position. Test coupon size is 12mm thk and 300mm long.

Please give reference also.

 

Thanks to all for your valuable inputs.
Thanks,
With Best Regards,
Ramesh Barot

Cell+919978917399

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...