Yes
        as per ASME SEC IX - EDITION 2010  QW-142 , you can also qualify a welder by UT instead of RT.




with regards

SOUMYAKANTA MAHALIK
(Mechanical Engineer with spl. in welding technology)

On 30 March 2011 18:28, Ramesh Barot <rameshnbarot@yahoo.com> wrote:
Dear all experts,
 
Can we qualify welder by UT?

 
Thanks,
With Best Regards,
Ramesh Barot

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...