No , You cant go for directly CSWIP 3.2 ...

Refer www.twi.co.uk

Regards

Suresh

On 3/24/11, vijay <vijayakumarme@gmail.com> wrote:
> Hi Friends,
>
> As this query is related to certification , I can also ask post my doubts.
> Is it possible to do CSWIP3.2 certification directly without having
> CSWIP3.1? If possible what are the eligible criteria's
>
> Regards,
> Vijay
>
> On Thu, Mar 24, 2011 at 2:38 PM, Arun Das <indhuarun@yahoo.co.in> wrote:
>
>> Some clients in middle east countries are looking for CSWIP certified
>> inspectors.
>>
>> regards,
>>
>> Arun S Das
>>
>>
>> ------------------------------
>> *From:* Suresh <bobsuresh24@gmail.com>
>> *To:* materials-welding@googlegroups.com
>> *Sent:* Thu, 24 March, 2011 10:58:56 AM
>> *Subject:* Re: [MW:10469] AWS CWI Vs CSWIP 3.1 welding inspector
>>
>> AWS is which is organized by US Institute ...
>>
>> CSWIP is which is organized by UK based ....
>>
>> Both are equalant in terms certification.....but preference is always
>> based on company's/ Client recommendations...
>>
>> In best of my view is generally AWS is prefered in all over in the
>> world..all ASME codes are related to AWS ..
>>
>> Thank you
>>
>> Suresh
>>
>> On 3/24/11, U WYNN-NAING <u.wynn-naing@total.com> wrote:
>> > Hi,
>> >
>> > Can anybody explain the differences and advantages Between AWS CWI
>> welding
>> > inspector and CSWIP 3.1 welding inspector.
>> > Which course should I choose.
>> >
>> > Thanks and Rgds,
>> >
>> > WN
>> >
>> > --
>> > To post to this group, send email to materials-welding@googlegroups.com
>> > To unsubscribe from this group, send email to
>> > materials-welding+unsubscribe@googlegroups.com
>> > For more options, visit this group's bolg at
>> > http://materials-welding.blogspot.com/
>> > The views expressed/exchnaged in this group are members personel views
>> and
>> > meant for educational purposes only, Users must take their own decisions
>> > w.r.t. applicable code/standard/contract documents.
>> >
>>
>>
>> --
>> Thanks & Best Regards,
>>
>> Suresh
>>
>> Mobile No: 91-92 92 905 905
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to materials-welding+
>> unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>> --
>> To post to this group, send email to materials-welding@googlegroups.com
>> To unsubscribe from this group, send email to
>> materials-welding+unsubscribe@googlegroups.com
>> For more options, visit this group's bolg at
>> http://materials-welding.blogspot.com/
>> The views expressed/exchnaged in this group are members personel views and
>> meant for educational purposes only, Users must take their own decisions
>> w.r.t. applicable code/standard/contract documents.
>>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Thanks & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...