Re: [MW:10462] Pipe range Qualified

Dear Mr. Venkat,

This is referance to ASME Sec IX, QW-451,

Welder is qualify 2T when welder qualified thickness of test coupon
between 1.5 to 10 mm.

The qualified range of welder is 16 mm for 8 mm thk.

Dear experts,

Please revert if my understanding is wrong.

With Regards,
Vikas Rana

On Wed, Mar 23, 2011 at 12:57 PM, Venkateswaran
<k.venkateswaran@ionexchange.co.in> wrote:
> Regading the PQR/WPQ,if the welder Qualified in 1G position in 8 mm thck
> plate full penetration welding,what will be the qualified range in pipe .
>
> regards,
> kvr
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...