Wednesday, March 23, 2011

Re: [MW:10457] A No.

Thanks.
 
Let me clarify further.
 
I agree that A No needs to be mentioned in PQR but,
 
Is it required to carry out weld metal chemical analysis and describe the chemistry in PQR? Is any requirements mentioned in ASME B 31.3 regarding this?
Reg,
JJ
On Wed, Mar 23, 2011 at 11:47 AM, Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
Since the PQR is qualifying as per ASME Sec. IX, you have to mention the 'A' number in PQR.

Thanks & Regards
Muhammed Ibrahim PK



On 23 March 2011 08:43, joshi jaydeep <jaydeep.p.joshi@gmail.com> wrote:
Does Weld Metal Chemical analysis (A No.) is an essential to be mentioned while qualifying PQR for meeting ASME B 31.3?
 
Please let me know the clause if possible mentioning the above details.
 
 
Regards,
Jaydeep

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...