Hi,
When combination WPS,Base metal range will not be limited for each process.But weld metal thickness is limited

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Sat, 3/19/11, Sundaram Elumalai <Elumalai.Sundaram@starfab.com.sa> wrote:

From: Sundaram Elumalai <Elumalai.Sundaram@starfab.com.sa>
Subject: [MW:10434] process thk -AWS
To: materials-welding@googlegroups.com
Date: Saturday, March 19, 2011, 5:09 PM

Dear Mr.Karthikeyan,

 

Please give me your opinion for the following.

 

Recently we have qualified one PQR with

 

SMAW – Root and HOT pass.

FCAW –  Fill and Cap.

Base Metal thickness: 25.4mm / 10" Pipe Dia

Code : AWS D1.1,2010.

SAES-W-013.

 

Since SAES-W-013 Clause 5.4.2 is confirming that FCAW process shall not be used for Root and we have followed the same condition during the PQR qualification.

 

 

Our interpretations are as follows:

 

1.       As per the AWS D1.1, Table 4.2 - If we use the plate thickness of 25mm over, qualification range will be 10mm to unlimited.

2.       I have stated in the WPS that SMAW process is only for root and hot pass and FCAW for FILL &CAP.

3.       Based on the SAES-W-013 and AWS Table 4.2, the QUALFICATION range for the WPS is 10mm to unlimited or 0.5 to 1.5 of base metal thickness.

4.       For the combination of Welding Process ( SMAW+FCAW), The thickness limitations will not be applicable for each process since root and Hot Pass of SMAW is not for FILL & CAP

5.       SMAW WELD METAL is backing for FCAW.

6.       We always use the WPS as SMAW –ROOT /HOT Pass & FCAW – FILL&CAP.

 

Clarification required:

 

1.       For the combination of welding process, the thickness limitation will not be for each process.

2.       Base metal Qualification range will be considered for both the process. ( as below).

 

 

 

With Kind regards,

 

S.Elumalai.

******************************************************************************************
CONFIDENTIALITY NOTICE
This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...