Thursday, March 31, 2011

[MW:10546] Wire and Flux

Dear All,
 
1- I want to know suitable combination between wire and Flux for welding Stainless Steel material by SAW process
SA 240 Tp 304L and please give AWS classification for both.
 
2- suitable steps for welding

--
Best Regardes,

 
 

Eng:- Elsayed Elghareeb.
Dipl. Welding Engineer.
+2 010 82 61 645.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...