Dear Ramesh Barot,

 

Yes. As per ASME Sec IX 2010 edition with reference to the following

 

Refer list of changes and record number 08-1330 along with

 

Refer QW 142, 143 , QW-191.2.1 & QW-302.2

 

It states UT can be conducted on test welds in material ½ “ (13mm) thick or greater

It shall be done with written procedure verified by the manufacturer to be in compliance with T-150 of sec V ( which states about a written procedure and demonstration…)

 

Hope this is helpful

 

Cheers

MM

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ramesh Barot
Sent: Wednesday, March 30, 2011 4:58 PM
To: Materials Welding
Subject: [MW:10529] Welder Qualification

 

Dear all experts,

 

Can we qualify welder by UT?


 

Thanks,
With Best Regards,
Ramesh Barot

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...