Wednesday, March 30, 2011

[MW:10526] Re: Effect of Slope on Projection and Elevation of Nozzle during Pressure Vessel Fabrication

MIM,
Its actually tilt of the flange face & must be in deg ( usually 0.5˚),
not in %. If tilt is excessive, the effect would have major influence
on gasket fit mainly on to the connections to be fixed on the site.
However, it can be conpensated at site, since the connection at site
will have flange not welded usually.

Regards,
Bali Naushad


On Mar 29, 11:03 am, Idris Mohiuddin <idrism...@gmail.com> wrote:
> Dear Experts,
>
> Please throw some light on the following query:
>
> :What effect will Slope have on projection & Elevation of Nozzle during
> fabrication of Pressure Vessel (Slope is given as 1.5% in GA Drawing)"
>
> Regards,
>
> MIM

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...