Monday, March 21, 2011

[MW:10451] RE: 10450] Crack in the welding of SA516-70 DISH END and 316L nozzle

Dear Mr Shamesh,

 

Please arrange to forward the joint sketch (joint preparation) and WPS for analyses to comment on the solution.

 

Regards,

 

C.Nagabhushanam

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of shamesh Lotlikar
Sent: Monday, March 21, 2011 11:24 AM
To: materials-welding@googlegroups.com
Subject: [MW:10450] Crack in the welding of SA516-70 DISH END and 316L nozzle

 


Dear ALL,

We are manufacturing vessel which is claded with 316L and on the dish end of material SA516-70 and nozzles welded in double bevel weld joint. when completed one side of welding. We did carbon arc gouging and done magnetic particle test and we found cracks at toe of welding on side of 316L nozzle side. We used 309L-16 electrode. The wall thickness of nozzle is around 25 to 30mm and dish end material SA516-70. I would like to know what procedure to be used for repairing the crack and is it we have change the electrode to E312-16. Kindly advice or if any technique of welding to repair and do complete  

regards
shamesh

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...