Date: Mon, 21 Jun 2010 04:45:24 -0700
From: kashkousha1@yahoo.com
Subject: Re: [MW:5682] weld SA-106 to 9 Cr materials P No 5B gr 1 or gr 2
To: materials-welding@googlegroups.com
dear ahmed
yes,by using ER 90S-B9(GTAW)&E9018-B9 (SMAW) or E 9015-B9
the joint should be heat treated acc .to ASME B31.3
H.KASHKOUSHA
From: Ahmed Hafez <diesel2002@hotmail.com>
To: Welding Material <materials-welding@googlegroups.com>
Sent: Mon, June 21, 2010 1:42:17 PM
Subject: [MW:5681] weld SA-106 to 9 Cr materials P No 5B gr 1 or gr 2
good morning every one
is it applicable to weld SA-106 to 9 Cr materials P No 5B gr 1 or gr 2
thanks and best regard
Your E-mail and More On-the-Go. Get Windows Live Hotmail Free. Sign up now.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
yes,by using ER 90S-B9(GTAW)&E9018-B9 (SMAW) or E 9015-B9
the joint should be heat treated acc .to ASME B31.3
From: Ahmed Hafez <diesel2002@hotmail.com>
To: Welding Material <materials-welding@googlegroups.com>
Sent: Mon, June 21, 2010 1:42:17 PM
Subject: [MW:5681] weld SA-106 to 9 Cr materials P No 5B gr 1 or gr 2
good morning every one
is it applicable to weld SA-106 to 9 Cr materials P No 5B gr 1 or gr 2
thanks and best regard
Your E-mail and More On-the-Go. Get Windows Live Hotmail Free. Sign up now.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Hotmail: Free, trusted and rich email service. Get it now.
No comments:
Post a Comment