Dear Amit,
You can try Silicon Aluminium paint which can resist the tempreature upto 400 degreee C
if applied directly without primer coat.
if applied directly without primer coat.
Ameron 878 is the paint
Ravimenon.
Bahrain
From: AGUSTIN JIMENEZ <agumarca@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Sun, 20 June, 2010 6:20:22 AM
Subject: Re: [MW:5661] Paint for Aluminum Heat Exchangers
Hi.
Is recommendable not paint, if you paint you will have problem with temperature interchange.
AGUSTIN JIMENEZ
De: "amitrunsworld@gmail.com" <amitrunsworld@gmail.com>
Para: Materials & Welding <materials-welding@googlegroups.com>
Enviado: vie, junio 18, 2010 1:09:21 PM
Asunto: [MW:5651] Paint for Aluminum Heat Exchangers
Dear Group Members,
Could you please guides which type of paint we can use for general
application for corrosion protection purpose for aluminum heat
exchanger used as an Engine Radiator, Transformer oil cooler, Oil
coolers for locomotives working temperature up to 150C.
Thank you
Amit
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment