i would be thankful if answer to my question:
,as ASTM_ A105 are the elements Ni, Cr,Mo, Cu, Nb essential elements
or not .
I means in the material certificate ,the chemical composition for
above elements necessary must be report or not??

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements