Sorry, I did not see the items for which this is used. For valves, it is acceptable to use ASTM, in place of SA.
arun

On Tue, Mar 9, 2010 at 8:15 PM, Arunachalam A <arunvani@gmail.com> wrote:
if the item SA 216 is meant for code stamped vessels and parts, then the acceptable ASTM editions are upto 2007 editions ( check the table of acceptable ASTM Editions in Part II-A).
You need to check the material certificates, if the same is of ASTM. If ASTM is mentioned in the MTC, instead of SA, then ASTM EDITION Year need to be in Certificate.

arun


On Tue, Mar 9, 2010 at 6:59 PM, John Henning <jhenning@deltak.com> wrote:
SA-216 states the following:  "Identical with ASTM Specification A216/A216M-07 except for the addition of 2.3 and editorial differences in 2.1 and 10.1."
 
2.3 references ASME Section IX
10.1 requires welders and welding procedures used for repair to be qualified in accordance with ASME Section IX
 
 2.1 - no significant difference that I could quickly discern
 
All else is the same.
 
John

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of vijay frnds
Sent: Tuesday, March 09, 2010 3:13 AM
To: materials-welding@googlegroups.com
Subject: [MW:4502] ASTM A216 Vs ASME SA216 Difference

Dear friends,


I have received the customer order for pipeline valves with ASME SA216 Gr WCB.

My doubt is there any diff. between ASTM A216 Gr WCB Vs ASME SA216 Gr WCB.

Thank you,


--
Urs . . .
Muthu
Smile make(s)miles ! ! !
Please don't print this e-mail unless you really need to! - this will preserve trees on our planet earth.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
ARUNACHALAM.A
050-5257122

There are three types of people in the world,
First makes wonder happen,
Second see wonders happen and
Third one wonders what happened!



--
ARUNACHALAM.A
050-5257122

There are three types of people in the world,
First makes wonder happen,
Second see wonders happen and
Third one wonders what happened!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...