Friday, March 5, 2010

Re: [MW:4436] ultrasonic testing method LIMITATIONS

I have tested successfully from 7 - 240mm.
 
In your case 30mm is no problem at all. (I belive scanning access is perfect)
 
S.Senthilkumar

--- On Fri, 5/3/10, hwjoshi@tce.co.in <hwjoshi@tce.co.in> wrote:

From: hwjoshi@tce.co.in <hwjoshi@tce.co.in>
Subject: [MW:4429] ultrasonic testing method LIMITATIONS
To: materials-welding@googlegroups.com
Date: Friday, 5 March, 2010, 11:21 AM


upto what thickness of the weld joint can ultrasonic testing method work successfully?

i have a butt weld  joint on two SA515  plates of thickness over 30mm.








your truly
H W JOSHI
ENGINEER MECHANICAL
TATA CONSULTING ENGINEERS LTD
MUMBAI - 400 013
TEL : 022 66624743 EXT : 127
---------------------------------------------------------------------------------------------------------- Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.  Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.  While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.  ---------------------------------------------------------------------------------------------------------  
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...