Are you talking about Stainless or similar materila ?
Regards, jimmy
On 5 March 2010 12:26, raw <rohit30584@gmail.com> wrote:
> Hi there,
> I have a query related to the colour of welding.Sometimes the colour
> of welding comes out bluish and sometimes yellowish blue .Is this a
> kind of welding defect or anything else?
> Rohit Rawat,
> Asst. Engineer(QA),
> Kirby Building Systems,Haridwar.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com