AWS D1.1 I based off of the defect point system. DAC or TCG are not acceptable.
From: Ali Asghari <asghariali@rocketmail.com>
To: materials-welding@googlegroups.com
Sent: Wed, March 3, 2010 6:05:32 AM
Subject: [MW:4407] evaluating based on AWS D1.1 for UT
Dear All
what is the sensitivity refrence line for ultrasonic testing according AWS D1.1?
is DAC applicable?(if yes, in which paragraph this refered?)
regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.