[MW:4403] Heat treatment of materials/flanges

1. In pressure vessel steel plates-SA 516 Gr70MT here what is the
meaning of MT, is it any additional heat treatment other than
normalized? some plate MTCs are showing tensile/Yield values after
stress relieved/PWHTed? Is it a code requiement- if it so the holding
temp & time information where I will get (for SA 516Gr 70 material &
SA105/SA350LF2CL1)? Is it like SPWHT of Cr-Mo steels (ASME Sec VIIID2-
3.4 Supplemental Requirements for Cr–Mo Steels). Why SPWHT is required
for Div 1 construction even though we have PQR/WPS for the welding?

2. And for hot tensile test what is the prescribed temperature for
test? Is it a code requirement?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...