Dear All, Why we go for 0.1% & 0.2% offset method for physical testing of some metals? Does it realy makes the diff? Pl. reply psp |
The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.
Dear All, Why we go for 0.1% & 0.2% offset method for physical testing of some metals? Does it realy makes the diff? Pl. reply psp |
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...