[MW:3641] Re: Vent hole

Dear Bharat,
If the doubler plates need not be pneumatic Tested, then you can make a vent hole for escaping the gases during welding. And when the seal welding completed then plug this hole with insert, weld the same and ground flush with MT or PT.
 
Regards,
Nilesh Pathare

On Wed, Nov 11, 2009 at 12:29 PM, daniel iordache <daniel.iordache@gmail.com> wrote:
Hi
generally for small plate attachment .....where the shell is not penetrated is not necessry tale hole....the internal pressure acumulated during welding is quite small.....but as you said the is better as per engineering recomandation
for nozzles reinforcement we do also pneumatic test ....on that tale hole.....
 
regards


 
On Wed, Nov 11, 2009 at 6:10 AM, BHARAT GOLE <bharatgole@hotmail.com> wrote:
We are constructing tank as per API 650 & tell tale hole is required for reinforcing plate for all opening as per code.
But how about doubler plates and supports which will be permanent attachments on shell. I know tell tale hole is not required for leak test but at least vent hole is reqd as per good engg practice.But API 650 is silent on this issue.
Please suggest
Regards

Bharat B. Gole





http://windows.microsoft.com/shop Find the right PC for you.




--
Daniel Iordache
Bureau Veritas - Angola
Mechanical& Welding Surveyor
Mobile Ao: +244921544583
Mobile Ro:   +40721731728
E-Mail: daniel.iordache@gmail.com
          daniel_iordache@yahoo.com







--
Best Regards,

Nilesh Pathare

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...