[MW:3596] Re: 3582] Minimum Distance Between two welds

Dear Prapulla,
 
Is not suitable that 2 welds share a HAZ, since that the minumun distance should be  2 times HAZ.
 
BR
 
AV
 

 

Date: Thu, 5 Nov 2009 12:12:03 +0400
Subject: [MW:3595] Re: 3582] Minimum Distance Between two welds
From: gpadmana@gmail.com
To: materials-welding@googlegroups.com

Dear Praphulla,
Distance between two  welds to be mentioned in Project specification of piping.None of the codes and standards specify this.
 

 

 
On Wed, Nov 4, 2009 at 10:31 PM, Minal Patel (Sorge's Welding) <mpatel@metalcare.com> wrote:

As long as their caps are not touching

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Phirke, Praphulla D
(GE Infra, Oil & Gas)
Sent: Wednesday, November 04, 2009 1:02 AM
To: materials-welding@googlegroups.com
Subject: [MW:3582] Minimum Distance Between two welds



Dear All,
Anyone know where I can find the minimum distance to be maintained
between two welds ?
Please let me know

Thanks
Praphulla




<br
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

2 comments:

Suresh Paidi said...

Hii ,

we should maintain min distance the reason is HAZ should not be overlaped and to avoid stress concentration ,In best of knowledge we have to mantain min 1 inch between seam to seam and seam to elbow and adjacent welds .

Suresh
Fluor

Suresh Paidi said...

Hii ,

we should maintain min distance the reason is HAZ should not be overlaped and to avoid stress concentration ,In best of knowledge we have to mantain min 1 inch between seam to seam and seam to elbow and adjacent welds .

Suresh
Fluor

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...