Dear Praphulla,
Distance between two welds to be mentioned in Project specification of piping.None of the codes and standards specify this.
On Wed, Nov 4, 2009 at 10:31 PM, Minal Patel (Sorge's Welding) <mpatel@metalcare.com> wrote:
As long as their caps are not touching
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Phirke, Praphulla D
(GE Infra, Oil & Gas)
Sent: Wednesday, November 04, 2009 1:02 AM
To: materials-welding@googlegroups.com
Subject: [MW:3582] Minimum Distance Between two welds
Dear All,
Anyone know where I can find the minimum distance to be maintained
between two welds ?
Please let me know
Thanks
Praphulla
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
No comments:
Post a Comment