[MW:2842] QUERY ON SUITABLE FILLER WIRE FOR INCONEL 600

REPLY DTD 28TH JULY 2009

DEAR SORIN STEFAN
YOU CAN USE AWS ERNiCr-3 GRADE (BRAND OF SPECIAL METALS IS INCONEL
82) FILLER WIRE. AVAILABLE FOR MIG/TIG AND ALSO SAW APPLICATION.
FOR WELDING GUIDELINES VISIT www.specialmetalswelding.com
THIS SITE HAS ALL THE INFO YOU WANT.
REGARDS

CHANDER C GIROTRA
MUMBAI/ INDIA
====================================================
On Jul 24, 7:36 pm, sorin stefan <ssori...@hotmail.com> wrote:
> Hi Guys,
>
> Please tell me what is the best match of the filer material and gas for welding ALLOY 600 ( plates 1/4"up to3/") using MIG and TIG procedures.
>
> If you also have some welding giudelines - welding procedure regardless, it will be great
>
> Getting an answer ASAP it will be very much apreciated
>
> Thanks a lot
>
> Sorin St.
>
> _________________________________________________________________
> Stay on top of things, check email from other accounts!http://go.microsoft.com/?linkid=9671355

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...