[MW:2817] Re: LTCS Welding

If impact test is required you can use 6013 up to -27 Degree not minus
33 Degree, Better to go for 7016 for root and E7018-1 for Fill and
cap.


Regards
Israr Ahmed
Sr.Engr. QA/QC
Algaswa.support co.Ltd. Jubail KSA


On Jul 25, 8:22 am, "Nikhil" <nikhilrp_2...@rediffmail.com> wrote:
> Dear Friends,
>
> I like to know whether we can use the combination of E6010 in root and E7018-1 as filler in LTCS (A333Gr6) welding, particularly in Ammonia service (flash point is minus 33 deg C)?
>
> The working temp is less than minus 33 deg C. At what temp should I impact test it?
>
> Regards,
>
> Nikhil
> QC Engineer
> Sharjah, UAE
> +97150 1453525

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...