Sunday, July 26, 2009

[MW:2814] Re: SA-276 type 316 Bar

Dear Mr Devang,

I have used welding on the same no problem faced


Regards

Israr Ahmed


On Jun 29, 1:06 pm, "Devang Patel" <deva...@inoxindia.com> wrote:
> I want to weld SS-304L cleat on it by GTAW.
>
> Regards,
>
> Devang Patel
> Manager Engineering
>
> INOX INDIA Ltd.
> Ph :+91-265-3056392-3056100
> Fax :+91-265-2333398-2341449
> email : deva...@inoxindia.comwww.inoxindia.com
>
>
>
>   ----- Original Message -----
>   From: Shashank Vagal
>   To: materials-welding@googlegroups.com
>
>   Cc: deva...@inoxindia.com
>   Sent: Monday, June 29, 2009 12:14 PM
>   Subject: Re: [MW:2570] SA-276 type 316 Bar
>
>         Devang,
>         What welding exactly you want to do here, if you could elaborate on that, the members will be in a better position to answer...
>         Rgds,
>         Shashank
>
>         --- On Mon, 29/6/09, Devang Patel <deva...@inoxindia.com> wrote:
>
>           From: Devang Patel <deva...@inoxindia.com>
>           Subject: [MW:2570] SA-276 type 316 Bar
>           To: materials-welding@googlegroups.com
>           Date: Monday, 29 June, 2009, 11:21 AM
>
>           We have a rod of SA-276 TP316 with Condition S, Some of my senior told, welding is not permitted on this rod but i have not found any restriction in ASME code.
>
>           Can anyone know about it?
>
>           Regards,
>
>           Devang Patel
>           Manager Engineering
>
>           INOX INDIA Ltd.
>           Ph :+91-265-3056392-3056100
>           Fax :+91-265-2333398-2341449
>           email : deva...@inoxindia.com
>          www.inoxindia.com
>
> ---------------------------------------------------------------------------­---
>   Love Cricket? Check out live scores, photos, video highlights and more. Click here.- Hide quoted text -
>
> - Show quoted text -

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---