Dye penetrant inspected prior to the start of repair welding is recommended in order to confirm the complete removal of defects...
PAN
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
PAN
2009/6/30 Nikhil <nikhilrp_2006@rediffmail.com>
Whether cracks observed in Seat or other part?
If in seat and if it is stellited, ou need to remove stellite before depositing fresh weld of stellite.
Nikhil
On Tue, 30 Jun 2009 12:18:08 +0530 wrote
>Dear all,
>
>Kindly advise repair of cracks observed in gate (overlay of satellite-6 on
>F-6 base material)
>
>Thanks,
>
>S.Waheedullah Shah
>
>
>>
>
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments