Thursday, May 28, 2009

[MW:2264] Re: about WQT

Definitely NOT POSSIBLE, Tamil!

You should use the same material (P45) only for welder qualification
also.

The range can be applied from P41 through P49 (not P1) with F Number
fixed

Thanks
Senthil


On May 27, 5:30 pm, tamizazagan nagappan <tamizazag...@gmail.com>
wrote:
> I have wps for P45 material incoloy 825 UNS -08825, ASTM SB 462/464 UNS
> (N08020) NACE with filler metal F43 SFA 5.14  AWS    Er-Ni-Cr-Mo-3...
>
> Is it possible to qualify the welder with A333 Gr 6 base metal  with filler
> metal F43  SFA 5.14  AWS    Er-Ni-Cr-Mo-3...
>
> --
> TAMIL
> phone: +77023210394
>
> --
> TAMIL
> phone: +77023210394
>
>  Save a tree...please don't print this e-mail unless you really need
> toRegards

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS