[MW:2130] Re: Drain plug material

Similar forged material is A105

fga

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of vijay frnds
Sent: sexta-feira, 8 de Maio de 2009 6:14
To: materials-welding@googlegroups.com
Subject: [MW:2127] Drain plug material

 


Can any one tell me What is the drain Plug Material For Astm A216 Gr WCB.

--
Urs . . .
Muthu
Smile make(s)miles ! ! !
Please don’t print this e-mail unless you really need to! - this will preserve trees on our planet earth.
Clarence Darrow  - "When I was a boy I was told that anybody could become President; I'm beginning to believe it."


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...