How thick is the duplex, what film are they using and what source 
From: "Chaitanya Purohit"
Date: Fri, 27 Mar 2009 11:03:30 +0800
To: <materials-welding@googlegroups.com>
Subject: [MW:1813] RT of Duplex Stainless Steel
     
***DISCLAIMER NOTICE ***
"This email and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above. If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited. If you receive this email in error, please notify the sender immediately by return email and delete the email and any of its attachments. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."
 
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
 
Sent from my Verizon Wireless BlackBerry
From: "Chaitanya Purohit"
Date: Fri, 27 Mar 2009 11:03:30 +0800
To: <materials-welding@googlegroups.com>
Subject: [MW:1813] RT of Duplex Stainless Steel
Dear All,
I am facing problem during NDT (RT) of Duplex St.Steel) . The RT film shows 4-5ā long white indication in the weld area. We tried changing the screen but still the same things appear on the film. 
The welds are welded with SAW process. Generally the porosities are expected if we use SAW welding for Duplex but this indications are strange for me. Does anybody have experienced the same ?
Regards.
 
C. K. Purohit
***DISCLAIMER NOTICE ***
"This email and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above. If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited. If you receive this email in error, please notify the sender immediately by return email and delete the email and any of its attachments. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments