[MW:1780] RE: 1779] Re: Equivalent for BS4360

Yes nearest ASTM equivalent will be A36, however this standard was officially withdrawn from 1994 and its current equivalent is Grade S275 (EN 10025 part 2)

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Vinod Upadhyay
Sent: Wednesday, March 18, 2009 9:09 AM
To: materials-welding@googlegroups.com
Subject: [MW:1779] Re: Equavalent for BS4360

 

ASTM A36 can be used .

On Wed, Mar 18, 2009 at 9:58 AM, Kim <shihyuen81@gmail.com> wrote:


Dear All,

Good day to everybody.

I am thinking of using BS4360 Gr 43A material C-Channel to fabricate
as the skid base, but client would like to know the equalvalent for
this material in ASTM. I much appreciated anybody could advise this.

Thanks in advance.

Regards,
Kim SY





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...