Friday, March 13, 2009

[MW:1761] Re: Heat input during welding

You are right for its all so mentioned in ASME sec-IX


 
2009/3/13 Ayhan GEDUK <aygedik@yahoo.com>
Dear Akasy
There are a lot of project specification is different, but normally 10% of deviation from approved PQR but some of teh client spec. asking for max. 15%.
Regards,

Ayhan GEDUK

--- On Wed, 11/3/09, Ali Asghari <asghariali@rocketmail.com> wrote:

From: Ali Asghari <asghariali@rocketmail.com>
Subject: [MW:1756] Re: Heat input during welding Date: Wednesday, 11 March, 2009, 6:31 AM

seperate from qualified range,the heat input depends to current & voltage.therefore in gmaw transfer mode change.e.g from spray to short circuit or vice versa,affect on deposition rate & depth of penetration.


From: sandy kumar <sandy001987@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sunday, March 8, 2009 12:17:51 PM
Subject: [MW:1721] Heat input during welding

In GMAW what is the effect of heat input on weld? How much variation in hezt input is allowed above thw WPS qualifiedrange.
Please tell me
Akashy



Get your preferred Email name!
Now you can @ymail.com and @rocketmail.com





--
Regards

Rajeev Arora




"DON'T LET SOMEONE BECOME A PRIORITY IN YOUR LIFE...
WHEN YOU ARE JUST AN OPTION FOR THEM....."

SO , Always keep in mind that......

DON'T GO THE WAY LIFE TAKES YOU,
TAKE THE LIFE THE WAY YOU GO,

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...