[MW:1081] Re: Burmah-Castrol strip type 1

Field Flux Strips (Burma Castrol) Type I (G)eneral
&
Field Flux Strips (Burma Castrol) Type II (A)ircraft

Magnetic Flux* Strips are a simple-to-use, inexpensive and effective tool that provides you with assurance that you are performing an effective magnetic particle test.

 

Their proper use proves that you have:

- Adequate field strength and direction

- Proper illumination

- Appropriate magnetic particle properties

Magnetic Flux strips should be used to confirm that all required testing parameters, including: lighting, field strength and direction, magnetic particle properties and coverage are sufficient to find surface cracks equal or greater in size than those built into the strip. 

 

Magnetic Flux  Strips can be used with; Fluorescent, Wet Visible (Black & White) as well as Dry Particles (with or without contrast). They can be used with AC, FWDC and HWDC magnetization, with either longitudinal or circular fields. 

 

They can also be used to demonstrate the sensitivity differences between these methods and to develop magnetizing techniques and to assure complete coverage. 

 

They should be a mandatory part of all Magnetic Particle testing procedures.

 

* Previously known as "Burmah-Castrol" Strips. They are a form of Q.Q.I. and could replace "pie" gauges.



Bharat B. Gole

 

 




Subject: [MW:1080] Burmah-Castrol strip type 1
Date: Tue, 2 Sep 2008 16:51:44 +0530
From: R.Bathula@ticb.com
To: materials-welding@googlegroups.com

What is Burmah-Castrol strip type 1?  And how sensitivity will be demonstrated in MT with this?

 

 





MSN Technology brings you the latest on gadgets, gizmos and the new hits in the gaming market. Try it now!
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Anonymous said…
Your blog keeps getting better and better! Your older articles are not as good as newer ones you have a lot more creativity and originality now keep it up!

Popular posts from this blog

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...