Friday, October 7, 2016

Re: [MW:25496] GMAW for CS

Use 100% CO2 shielding gas with proper heater and gas flow rate.

Prem Nautiyal 




Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: 'MAGHROUD Moussa' via Materials & Welding <materials-welding@googlegroups.com>
Date: 03/10/2016 2:15 p.m. (GMT+05:30)
To: materials-welding@googlegroups.com
Subject: [MW:25476] GMAW for CS



Dear experts

I am trying to qualify a PQR using GMAW applied on a plate spec A36,10 mm thick, ER 70S6 1.2 mm, position 3G, progression downhill and Argon pure as shielding gas. But after RT shooting we find porosity throughout the joint. 
Please anyone can help how to qualify this weld. 


Envoyé depuis un mobile Samsung

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...