What is the max. nominal thickness of weld involved in skirt support ?
Regards
Prem Nautiyal
9769316004
--------------------------------------------
On Mon, 8/31/15, Shadab Ansari <shadabansarialam@gmail.com> wrote:
Subject: Re: [MW:23374] PWHT requirement for vessel
To: materials-welding@googlegroups.com
Date: Monday, August 31, 2015, 9:36 PM
No. Since its a
non-pressure part.
On Aug 29, 2015 5:04 PM,
"Prasad" <prsgne@gmail.com>
wrote:
Construction Code ASME Sec. VIII
Div. 1 Edn. 2013
Non pressure Part skirt support
of vertical vessel not welded directly to vessel.
MOC IS 2062 P no.1 Group 1
Thk. 40 mm
No special service requirement.
For this case whether PWHT is mandatory?
Regards,
Prasad G.
--
You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d725eb3d-aca0-435c-ba4c-feadeba7f303%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the
Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails
from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BEkGZc7hH9jjr5xvft3Oyfx3XYxTQ1Pc-7xwuD_KFs-Sj3DKQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1441302561.90531.YahooMailBasic%40web142701.mail.bf1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
[MW:34919] Welder qualification certificate
Dear All anyone can share a format for welder certificate and card format Thanks & Best Regards Saleem manhappulath Mob:+9665...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...