Dear Mr Rafeeq Ur Rahman.
We have 2 x 1000 TPD Sufuric Acid Plants, 750 MTPD Phos Acid Plant, 16x2 MW CPP & Wide HP & LP Stream distribution network.
We are facing Frequent acid , gas , steam leakages.
Any hot tapping procedure , that cal help us to carry out on stream, will be welcome.
Pl. let us know in return mail.
Regds,
akpradhan
From:
Sent: Saturday, May 05, 2012 2:58 PM
To:
Subject: Re: [MW:14190] HOT TAPPING OF LPG PIPE LINES
Dear Venkat,
recently we have done the Hot-tap for our project, the hot tap crew & their safety team will assess the area, condition of the site, as well as your emergency contingency plan based on the risk assessment.
you need to have basically following in your hand.
1) Hot-Tap package (hot-tap procedure, welding procedure, hot-tap calculation, UT reading, ISO, P&ID, MTO etc).
2) Emergency contingency plan.
3) Split tee hydro test reports.
4) Spool hydro test report. etc.
Warm Regards'
Rafeeq Ur Rahman
From:
To: materials-welding <
Sent: Thursday, 3 May 2012 11:16 AM
Subject: [MW:14177] HOT TAPPING OF LPG PIPE LINES
Dear Friends,
We are planning to do hot tapping of LPG pipe lines with wall thcikness of 9 mm. Does any body have experience with the same, please share. We have qualified the procedure, but there are apprenhensions regarding safety in hot tapping of LPG pipe lines
Regards
Venkat
--
To post to this group, send email to
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
1 comment:
Please contact us for more details. We will provide you all details & service in this regard.
Regards / S. Wani
shw@conmatindia.com
Post a Comment