Dear Dokku
The standards and their editions as listed in table U-3 are mandatory. They could vary from section to section.
Espacially for the SNT/TC/1A, the section VIII div 1 refers to older editions (when you compare the various editions and addenda´s), whilst section I refers to newer editions of this standard.
Regards
Fred Bosman
Op 15-3-2011 12:39, DOKKU AJAY schreef:
The standards and their editions as listed in table U-3 are mandatory. They could vary from section to section.
Espacially for the SNT/TC/1A, the section VIII div 1 refers to older editions (when you compare the various editions and addenda´s), whilst section I refers to newer editions of this standard.
Regards
Fred Bosman
Op 15-3-2011 12:39, DOKKU AJAY schreef:
Dear Experts,ASME Sec.VIII Div.1 Tbale U-3 refers to some older editions of standards for which the latest editions are available.For eg: SNT-TC-1A latest edition is 2006. However, Table U-3 refers to 2001 Edition.1. Is it acceptable to use latest standards?2. If Yes, then, do we have any interpretaion for this?Thanks,Dokku Ajay Kumar
Mobile: +966 500071054
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/