Dear Muthu Bharathi
 
Table 2 is only for the specimens requirement for pqr as per dia .its does't say that range of qualification. Iam right?
According to 5.3.2.3 wps need to show only the dia inch as per grouping of 6.2.2
according to 5.4 essential variables does't say that dia is essencial variable only there is mensioned that the wall thickness in 5.4.2.5
as of my interpritation if the thicness with in the group wecan use the procedure for production weld irrespective of size
 
pls let me know if iam wrong
 
 


 
On Sun, Mar 13, 2011 at 12:51 AM, muthu barathi <muthu_barathi@rediffmail.com> wrote:


Dear Sir,

You may please refer Table 2 of API 1104 and from this table you may find diameter range and wall thickness range. you mentioned only dia and not wall thk. if the wall thk is as 20" dia  or with in 0.5" you may use the same PQR.



Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

On Sat, 12 Mar 2011 21:44:08 +0530 vijay kumar <vijaykumaar80@gmail.com> wrote

>Dear All,
>
>i have a pqr 20" thk 11.91 mm as per api1104 ,for the production weld
>we can apply this to 10" pipe of same grade material.
>
>--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...